C | Cr | Cu | Mn | Mo | Ni | P | S | Si |
Max | Max | Max | Max | Max | ||||
0.02 | 19.0-23.0 | 1.0-2.0 | 2.0 | 4.0-5.0 | 23.0-28.0 | 0.045 | 0.035 | 1.0 |
GANPAT METAL INDUSTRIES - | E-Showroom
GANPAT METAL INDUSTRIES - | E-Showroom
904L Chemical Composition %
C | Cr | Cu | Mn | Mo | Ni | P | S | Si |
Max | Max | Max | Max | Max | ||||
0.02 | 19.0-23.0 | 1.0-2.0 | 2.0 | 4.0-5.0 | 23.0-28.0 | 0.045 | 0.035 | 1.0 |
Typical Applications Production and transport of sulfuric acid Metal pickling in sulfuric acid Production and concentration of phosphoric acid Use in seawater, brackish water, condensers, heat exchangers and pipe work in general Paper and allied industries Gas washing Chemical and pharmaceutical industries
Tensile requirements Tensile Strength (KSI) 70 Yield Strength (KSI) 25 KSI can be converted to MPA (Megapascals) by multiplying by 6.895.